1. Quantity adding of different vulcanizing and molding conditions
Vulcanizing | DCBP | DBPMH | BTS-510 |
Dosage | 1% | 1% | 3.5% |
Molding condition | 120℃*5 min | 170℃*10min | 120℃*5 min |
2. Quantity adding of different vulcanizing and extruding condition
Components | BTS-518 A | BTS-518 B |
Appearance | Yellowish transparent | Semi-transparent |
Mix ratio | 0.8-1.0% | 1.8-2.2% |
Molding condition | 120℃*5min |
3. Molding processing– Mix rubber until the smooth edge and the surface of the rubber are formed by double roller mill. Then fully mix it with a certain amount of vulcanizing and discharge it for use
4. The molding or extruding condition can be adjusted according to the dimension of the product